Manufacturing process of a para-aramid filament yarn, dyed in mass, and a wick, wick, staple fiber yarn and textile fabric

机译:批量染色的对位芳纶长丝纱线以及灯芯,灯芯,短纤维纱线和纺织面料的制造工艺

摘要

Process for manufacturing a dyed para-aramid filament yarn, in which the process comprises the steps of a) preparing a spinning paste comprising a para-aramid polymer, at least one dye and concentrated sulfuric acid , b) spin the spinning paste through a row to obtain spun filaments, c) coagulate the spun filaments to obtain coagulated filaments, d) neutralize the coagulated filaments to obtain neutralized filaments, e) wash the neutralized filaments to obtain washed filaments , and f) drying the washed filaments to obtain dry filaments, characterized in that in step a) the spinning paste is prepared with between 17.5 and 18.5% by weight of a para-aramid polymer with respect to the weight of the spinning paste and between 4 and 15% by weight of at least one dye with respect to the weight of the para-aramid polymer plus the at least one dye, and in step f), during drying, the fi Laments are kept under a tension in the range of 0.2 to 0.8 cN / dtex
机译:用于制造染色的对位芳族聚酰胺长丝纱线的方法,其中该方法包括以下步骤:a)制备包含对位芳族聚酰胺聚合物,至少一种染料和浓硫酸的纺丝浆料,b)将纺丝浆料纺成一排为了获得纺成的长丝,c)使纺成的长丝凝固以获得凝结的长丝,d)中和凝结的长丝以获得中和的长丝,e)洗涤中和的长丝以获得被洗涤的长丝,以及f)干燥洗涤的长丝以获得干燥的长丝,其特征在于,在步骤a)中,以相对于纺丝浆料的重量为17.5至18.5%重量的对芳族聚酰胺聚合物和相对于纺丝浆料的重量为4至15%的至少一种染料制备纺丝浆料。到对位芳族聚酰胺聚合物加至少一种染料的重量,并在步骤f)中,在干燥过程中,将纤丝保持在0.2至0.8 cN / dtex的张力下

著录项

  • 公开/公告号ES2635300T3

    专利类型

  • 公开/公告日2017-10-03

    原文格式PDF

  • 申请/专利权人 TEIJIN ARAMID GMBH;

    申请/专利号ES20140799458T

  • 申请日2014-11-18

  • 分类号D01F6/60;D01D5/06;D01D10/02;D01F1/04;D01F1/06;

  • 国家 ES

  • 入库时间 2022-08-21 13:35:08

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号