A method of preparing a nano-scale zero-valent iron, comprising the following steps: (1) adding, in an inert atmosphere, polyethylene glycol and deoxy ethanol to an aqueous solution of ferrous salt, and mixing; (2) mixing the solution obtained in step (1) with an alkaline aqueous solution containing boron hydride and performing a reduction reaction; (3) after the reduction reaction in (2) is complete, obtaining a precipitate; and (4) vacuum drying the precipitate to obtain nano-scale zero-valent iron. A surfactant combined with the prepared nano-scale zero-valent iron can markedly improve remediation efficiency of soil polluted with volatile organic compounds (VOCs).
机译:一种制备纳米级零价铁的方法,包括以下步骤:(1)在惰性气氛中将聚乙二醇和脱氧乙醇加入亚铁盐水溶液中并混合; (2)将步骤(1)中获得的溶液与含有氢化硼的碱性水溶液混合并进行还原反应; (3)在(2)中的还原反应完成后,获得沉淀; (4)将沉淀物真空干燥,得到纳米级零价铁。表面活性剂与制备的纳米级零价铁结合可以显着提高被挥发性有机化合物(VOC)污染的土壤的修复效率。

著录项

  • 公开/公告号WO2017008204A1

    专利类型

  • 公开/公告日2017-01-19

    原文格式PDF

  • 申请/专利权人 BEIHANG UNIVERCITY;

    申请/专利号WO2015CN83773

  • 发明设计人 SUN YIFEI;TIAN HUIFANG;ZHU TIANLE;

    申请日2015-07-10

  • 分类号B22F9/24;B09C1/08;

  • 国家 WO

  • 入库时间 2022-08-21 13:32:51

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号