Disclosed is a method for starting water spraying in copper sulphide ore heap bioleaching, comprising the following steps: 1) judging the feasibility of starting copper sulphide ore water spraying: if the acid production potential of the ore is greater than the acid consumption potential, water spraying is started; and 2) starting the water praying: moisturising is performed with water in the heap construction process of the copper sulphide ore, and after the completion of the heap construction, spraying is performed with water, when the pH value of a leach liquor 3.0, circulating spraying is performed, and when the pH value of the leach liquor is 3.0, acidophilus iron and sulphur oxidation microorganisms are inoculated in the leach liquor as a spraying liquor, and circulating spraying is continued, to gradually increase the concentrations of acid, iron and copper in the system solution, so that the starting of the copper sulphide ore heap bioleaching is achieved.
机译:公开了一种在硫化铜矿石堆生物浸出中开始喷水的方法,包括以下步骤:1)判断开始在硫化铜矿石喷水中的可行性:如果矿石的产酸潜力大于酸消耗潜力,则用水开始喷涂; 2)开始注水祈祷:在硫化铜​​矿的堆砌过程中用水进行保湿,堆砌完成后,当浸出液的pH值> 3.0时用水进行喷雾,进行循环喷雾,当浸出液的pH值<3.0时,将嗜酸铁和硫氧化微生物作为喷雾液接种在浸出液中,继续循环喷雾,逐渐增加酸,铁的浓度。以及系统溶液中的铜,从而实现了硫化铜矿石堆生物浸出的开始。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号