Provided is a glass that is for air-quench tempering and that, even when the glass is a thin glass that has a thickness of 2.5 mm or less, can have ample residual stress added thereto by air-quench tempering. A glass that is for air-quench tempering, that has an Fe3+ content, in terms of Fe2O3, of 2.2 mass% or more, that has an Fe2+ content, in terms of Fe2O3, of 0.8 mass% or less, that has an average thermal expansion coefficient α50-350 at 50℃-350℃ of 75×10-7/℃-90×10-7/℃, that has a glass transition point of 500℃-600℃, and that has, between the glass transition point and the yield point thereof, a maximum αmax thermal expansion coefficient of 410×10-7/℃ or higher.
机译:提供一种用于空气淬火回火的玻璃,即使该玻璃是厚度为2.5mm以下的薄玻璃,也可以通过空气淬火回火而添加足够的残余应力。用于空气淬火回火的玻璃,其Fe 3 + 含量(以Fe 2 O 3 表示)为2.2质量相对于Fe 2 O 3 ,Fe 2 + 含量为0.8质量%以下的Fe 50℃-350℃下的平均热膨胀系数α 50-350 为75×10 -7 /℃-90×10 -7 /℃,其玻璃化转变点为500℃-600℃,并且在玻璃化转变点与屈服点之间具有最大α max 热膨胀系数为410×10 < Sup> -7 /℃或更高。

著录项

  • 公开/公告号WO2017082312A1

    专利类型

  • 公开/公告日2017-05-18

    原文格式PDF

  • 申请/专利权人 ASAHI GLASS COMPANY LIMITED;

    申请/专利号WO2016JP83276

  • 发明设计人 HIJIYA HIROYUKI;MAEDA ERIKO;NAGAI KENSUKE;

    申请日2016-11-09

  • 分类号C03C3/085;B60J1;C03B27/04;C03C3/087;C03C3/089;C03C3/091;

  • 国家 WO

  • 入库时间 2022-08-21 13:31:03

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号