PFA PFA PFA MOLDED BODY WITH EXCELLENT BLISTER RESISTANCE AND METHOD OF CONTROLLING OCCURRENCE OF BLISTERS IN PFA MOLDED BODY
PFA PFA PFA MOLDED BODY WITH EXCELLENT BLISTER RESISTANCE AND METHOD OF CONTROLLING OCCURRENCE OF BLISTERS IN PFA MOLDED BODY
展开▼
机译:具有优异抗水泡性的PFA PFA PFA模制体以及控制PFA模制体中水泡发生的方法
展开▼
页面导航
摘要
著录项
相似文献
摘要
(Alkyl vinyl ether) having a melt flow rate of 0.1 to 100 g / 10 min as measured at a measurement temperature of 372 ± 0.1 ° C under a load of 5 kg according to ASTM D1238 There is provided a molded article having a hollow portion containing a copolymer of tetrafluoroethylene and perfluoro (alkyl vinyl ether), obtained by heat-treating a molded body having a hollow portion obtained by melt-molding a copolymer. The heat treatment is carried out at a temperature from the temperature 130 占 폚 lower than the melting point of the copolymer to the melting point of the copolymer. The shaped bodies exhibit excellent resistance to blistering under severe working conditions and when used in contact with harsh chemicals.
展开▼
机译:根据ASTM D1238在372±0.1°C的测量温度和5 kg的载荷下测得的熔体流动速率为0.1至100 g / 10 min的(烷基乙烯基醚)提供了具有中空部分的模制品含有四氟乙烯和全氟(烷基乙烯基醚)的共聚物,其是通过对具有通过将共聚物熔融成型而得到的中空部的成型体进行热处理而得到的。热处理在比共聚物的熔点低130℃的温度至共聚物的熔点的温度下进行。成型体在恶劣的工作条件下以及与苛刻的化学品接触时均表现出优异的抗起泡性。
展开▼