The present invention describes a cathode material for lithium ion batteries doped with Ni, Co-, and Mn-multi-elements with high compact densities and methods of making the same. The method for preparing the cathode material is as follows: (A) preparing an intermediate compound doped with Ni, Co-, and Mn-multi-elements by coprecipitation or chemical synthesis; (B) mixing the multi-doped intermediate compound with a lithium salt to prepare a mixture; (C) pre-treating the resultant mixture, then adding polyvinyl alcohol and uniformly mixing it; (D) pressurizing the resultant mixture into lumps, calcining at 800 to 950 占 폚, cooling outside, pulverizing, and passing through a 400 mesh sieve; And (E) calcining the resulting powder again at 700-800 占 폚, cooling it outside, grinding and sieving to obtain a product. The positive electrode material obtained by using a method described above has the general formula of LiNi x Co y Mn z M ( 1-xyz) O 2, in the range 0.6~30㎛ particle size, density of the compact 3.5~3.7g / ㎝ 3 , And can provide an initial discharge capacity of 150 to 165 mAh / g with excellent cycling and safety performance.
机译:本发明描述了一种用于锂离子电池的正极材料,该正极材料掺杂有高致密密度的Ni,Co和Mn多元素。制备正极材料的方法如下:(A)通过共沉淀或化学合成制备掺杂有Ni,Co和Mn多元素的中间化合物; (B)将多掺杂的中间体化合物与锂盐混合以制备混合物; (C)预处理所得混合物,然后加入聚乙烯醇并均匀混合; (D)将所得混合物加压成团块,在800至950占폚下煅烧,在外部冷却,粉碎,并通过400目筛网; (E)将所得粉末再次在700-800占占下煅烧,将其冷却至外部,研磨并筛分以获得产物。通过上述方法获得的正极材料的通式为 LiNi x Co y Mn z M( 1-xyz)O 2,其粒径在0.6〜30㎛范围内,密度为紧凑的3.5〜3.7g /㎝ 3 ,可提供150至165 mAh / g的初始放电容量,并具有出色的循环和安全性能。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号