The present invention relates to a reduced activation ferrite-martensite steel having excellent high resistance and a manufacturing method thereof, comprising: 0.08-0.12 wt% of carbon (C); 0.05-0.15 wt% of silicon (Si); 0.3-0.6 wt% of manganese (Mn); 8.7-9.3 wt% of chromium (Cr); 1.0-1.4 wt% of tungsten (W); 0.1-0.3 wt% of vanadium (V); 0.05-0.09 wt% of tantalum (Ta); 0.005-0.02 wt% of titanium (Ti); 0.005-0.02 wt% of zirconium (Zr); 0.005-0.015 wt% of nitrogen (N); 0.01-0.05 wt% of scandium (Sc); and the remaining consisting of iron (Fe).;COPYRIGHT KIPO 2017
机译:本发明涉及一种具有优异的高电阻的还原活化的铁氧体-马氏体钢及其制造方法,其包括:0.08-0.12wt%的碳(C);和0.05-0.15 wt%的硅(Si); 0.3-0.6 wt%的锰(Mn); 8.7-9.3 wt%的铬(Cr); 1.0-1.4 wt%的钨(W); 0.1-0.3 wt%的钒(V); 0.05-0.09 wt%的钽(Ta); 0.005-0.02重量%的钛(Ti); 0.005-0.02 wt%的锆(Zr);氮(N)0.005-0.015 wt%; 0.01-0.05 wt%的((Sc); ;其余为铁(Fe).; COPYRIGHT KIPO 2017

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号