FIELD: chemistry.;SUBSTANCE: water coating composition has the volume pigment content (VCP) from 70 to 78%, and contains, with respect to the total volume of solids in the dry coating: a) damping pigment particles comprising: i) from 4 to 10% of titanium dioxide, b) non-damping filler particles comprising: i) calcium and magnesium carbonate, and/or ii) calcium carbonate and/or iii) nepheline syenite, and/or iv) kaolin. The total content of i)+ii)+iii)+iv) is from 40 to 75%, and the content iv) is from 0 to 45% and contains c) particles of styrene-acrylic polymer binder, the glass transition temperature (Tg) of which, calculated by the equation of Fox, is equal from -30 to 5°C, and the acid number is from 15 to 65 mg KOH per 1 g of the polymer. The polymeric particles consist of acrylic monomers and optionally additionally comprise styrene derivatives; comprises d) a dispersing agent which is insoluble in water at pH 3; wherein the composition does not contain a volatile organic solvent and hollow polymer damping pigment particles. The method of covering the part, and the part or structure, the surface of which is covered by the claimed composition, are claimed.;EFFECT: water coating compositions provide improved abrasion resistance in the wet state.;19 cl, 1 tbl, 1 dwg
机译:领域:化学物质:水性涂料组合物的颜料体积含量(VCP)为70%至78%,相对于干涂料中的固体总体积包含:a)阻尼颜料颗粒,其包含:i) 4-10%的二氧化钛,b)非阻尼填料颗粒,其包含:i)碳酸钙和碳酸镁,和/或ii)碳酸钙和/或iii)霞石正长岩,和/或iv)高岭土。 i)+ ii)+ iii)+ iv)的总含量为40%至75%,iv)含量为0至45%,并包含c)苯乙烯-丙烯酸类聚合物粘合剂颗粒,玻璃化转变温度为(由Fox方程式计算的Tg为-30至5℃,酸值为每1g聚合物15至65mg KOH。聚合物颗粒由丙烯酸类单体组成,并且任选地还包含苯乙烯衍生物;优选地,苯乙烯类。包括d)在pH 3下不溶于水的分散剂;其中所述组合物不包含挥发性有机溶剂和中空聚合物阻尼颜料颗粒。要求保护覆盖零件的方法以及覆盖其表面被要求保护的组合物覆盖的零件或结构。效果:水性涂料组合物在湿态下提供了改进的耐磨性。19 cl,1 tbl,1 dwg

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号