首页> 外国专利> SHALE OIL DESULFURIZATION METHOD AND CATALYTIC OXIDATIVE DESULFURIZATION COMPOSITION FOR SHALE OIL

SHALE OIL DESULFURIZATION METHOD AND CATALYTIC OXIDATIVE DESULFURIZATION COMPOSITION FOR SHALE OIL

机译:页岩油脱硫方法及催化氧化脱硫组合物

摘要

FIELD: chemistry.;SUBSTANCE: method involves oil shale mixing in an organic solvent. At least 9 parts of an organic solvent are taken per one part of shale oil, the resulting mixture is oxidized by a catalytic oxidizing composition comprising hydrogen peroxide at a concentration of at least 50%, a salt selected from sodium molybdate, sodium tungstate, vanadyl sulfate, and an acid for oxidation reaction at the following ratio in molar proportions: salt selected from sodium molybdate, sodium tungstate, vanadyl sulfate:sulfur in oil = 1:500 to 1:50, hydrogen peroxide:sulfur in oil = 2:1 to 6:1, acid:sulfur in oil = 1:5 to 5:1. At that, 10 to 500 parts of the obtained mixture are taken per one part of the catalytic oxidizing composition, and the resulting mixture is treated at constant sonication power of 300 W for 2-6 hours, after which the solvent is removed and thermal cracking of the obtained mixture is carried out at 300-350°C for 3 to 6 hours.;EFFECT: objects allow to achieve a higher degree of sulfur removal.;12 cl, 3 ex
机译:领域:化学。物质:方法涉及在有机溶剂中混合油页岩。每一份页岩油至少取9份有机溶剂,所得混合物用催化氧化组合物氧化,该催化氧化组合物包含浓度为至少50%的过氧化氢,选自钼酸钠,钨酸钠,钒基的盐。硫酸盐和用于氧化反应的酸,其摩尔比例如下:选自钼酸钠,钨酸钠,硫酸氧钒:油中的硫= 1:500至1:50的过氧化氢:油中的硫= 2:1到6:1,油中的酸:硫= 1:5到5:1。此时,每1份催化氧化组合物取10至500份所得混合物,并将所得混合物在300W的恒定超声功率下处理2-6小时,然后除去溶剂并热裂解。所得混合物的混合物在300-350°C下进行3到6小时;效果:物体可以实现更高的脱硫率; 12 cl,3 ex

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号