FIELD: chemistry.;SUBSTANCE: lignin is pre-chlorinated with chlorine water. The resulting chlorlignin containing not more than 14.1% of chlorine is reacted with an alkali metal polysulphide which is obtained in an aqueous solution of hydrazine hydrate. The process of polycondensation at a temperature of 40°C and the molar ratio of chlorine to sulfur=1:1. The obtained product has a sorption value for nickel up to 360 mg/g, for zinc up to 423 mg/g, for cadmium up to 462 mg/g, for mercury to 467 mg/g, for copper 411 mg/g, for cobalt up to 323 mg/g, for lead to 376 mg/g.;EFFECT: improving the characteristics of the lignin obtained.;2 cl, 3 ex
机译:领域:化学。;物质:木质素已用氯水预氯化。使所得的含氯不超过14.1%的氯木素与在水合肼水溶液中获得的碱金属多硫化物反应。在40℃的温度和氯与硫的摩尔比= 1∶1的条件下进行缩聚反应。所获得的产品对镍的吸附值为360 mg / g,对于锌的吸附值为423 mg / g,对于镉的吸附值为462 mg / g,对于汞的吸附值为467 mg / g,对于铜的吸附值为411 mg / g。钴含量最高为323 mg / g,铅含量最高为376 mg / g;效果:改善了木质素的特性。2cl,3 ex

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号