FIELD: metallurgy.;SUBSTANCE: method for stabilising and inerting the slag includes the phases of introducing the components into the mixing device and the steps in which the slag is ground in a grinding device to produce particulate slag as particulate matter. The mixing means of the mixing device are activated. Pour the first amount of water into the mixing device. Waiting for the first period of time T1, beginning with the completion of the first water filling. Load crushed slag into the mixing device. Waiting for a second period of time T2, starting with the completion of slag loading into the mixing device. A hydraulic binder is introduced into the mixing device. Waiting for the third period of time T3, beginning with the completion of the loading of the hydraulic binder. A fluidifying additive is added to the mixing device. Waiting for the fourth time period T4, beginning with the completion of the loading of the fluidifying additive. A second amount of water is poured into the mixing device. Waiting for the fifth period of time T5, starting with the completion of pouring the second amount of water. The mixed product is withdrawn from the mixing device and the mixed product is maintained for a sixth period of time T6 or ripening time in a storage vessel with possible continuous or intermittent vibration to obtain an inert and mature product based on the slag. An inert and mature product is withdrawn from the storage container. Grind in a crushing device in order to achieve certain sizes of inert and mature product. In this case, a total amount of water corresponding to the sum of the first and second amounts of water is introduced relative to the total amount of components charged to the mixing device. Introduce slag, hydraulic binder and the fluidifying additive.;EFFECT: obtained product quality improvement.;20 cl, 2 dwg, 2 tbl
机译:技术领域:冶金学;物质:稳定和惰性化炉渣的方法包括将组分引入混合装置的阶段以及在研磨装置中将炉渣研磨以产生作为颗粒物的颗粒炉渣的步骤。混合装置的混合装置被激活。将第一批水倒入混合装置中。从完成第一次注水开始,等待第一时间段T1。将碎渣装入混合设备。等待第二时间段T2,从炉渣装载完成到混合装置开始。将水硬性粘结剂引入混合装置中。从完成液压粘合剂的加载开始,等待第三时间段T3。将流化添加剂添加到混合装置中。从完成流化添加剂的加载开始,等待第四时间段T4。将第二数量的水倒入混合装置中。等待第五个时间段T5,从第二个水的倒入完成开始。从混合装置中取出混合产物,并且将混合产物在储存容器中保持第六时间段T6或熟化时间,并可能进行连续或间歇振动,以获得基于炉渣的惰性且成熟的产物。从储存容器中取出惰性成熟的产品。在粉碎设备中进行粉碎,以达到一定尺寸的惰性和成熟产品。在这种情况下,相对于加入到混合装置中的组分的总量,引入与第一和第二水总量之和相对应的水总量。引入炉渣,水硬性粘结剂和流化添加剂。效果:产品质量得到改善; 20 cl,2 dwg,2 tbl

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号