FIELD: metallurgical engineering.;SUBSTANCE: method comprises preparing a mixture of purified titanium tetrachloride and purified vanadium tetrachloride. Purified vanadium tetrachloride is obtained by chlorinating the purified vanadium oxytrichloride with carbon tetrachloride. The ratio of the mixture of purified titanium tetrachloride and purified vanadium tetrachloride is maintained in the range 1:(0.7-1.0). In this case, the mixture is supplied for restoration first for one hour at a delivery rate of the mixture of not more than 100 kg/h and then at a delivery rate of not more than 150 kg/h. During the supply of the mixture, a constant temperature and a constant overpressure of argon are maintained. During the recovery, magnesium chloride is periodically drained off.;EFFECT: invention allows to obtain a doped sponge titanium homogeneous in composition, as well as with a given content of the alloying metal.;12 cl
机译:领域:冶金工程。物质:该方法包括制备纯化的四氯化钛和纯化的四氯化钒的混合物。通过用四氯化碳氯化纯化的三氯氧化钒获得纯化的四氯化钒。纯化的四氯化钛和纯化的四氯化钒的混合物的比例保持在1:(0.7-1.0)的范围内。在这种情况下,首先以不超过100kg / h的混合物的输送速率然后以不超过150kg / h的输送速率将混合物供应用于恢复一小时。在混合物的供应期间,保持恒定的温度和恒定的氩超压。在回收过程中,氯化镁会定期排出。效果:本发明可以得到组成均匀的掺杂海绵钛,并含有一定含量的合金金属。12cl

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号