首页> 外国专利> COATED ELECTRODE FOR LOW HYDROGEN TYPE FILLET WELDING

COATED ELECTRODE FOR LOW HYDROGEN TYPE FILLET WELDING

机译:低氢型角焊条的焊条

摘要

PROBLEM TO BE SOLVED: To provide a coated electrode for low hydrogen type fillet welding being excellent in welding workability such as a low fume generation rate and the like while ensuring excellent pit resistance, capable of obtaining excellent mechanical property of a weld metal and having good productivity.;SOLUTION: In a coated electrode for low hydrogen type fillet welding,: in mass% to the total mass of a coating agent, the total amount of metal carbonates is 5-15%; the total amount of metal fluorides is 3-8%; NaF in the metal fluorides is 0.2-1.5%; the total amount of TiO2 conversion values is 5-15%; the total amount of SiO2 conversion values is 10-20%; the total amount of Al2O3 conversion values is 0.5-3.0%; the total amount of FeO conversion values is 0.5-1.5%; MgO is 2-6%; Si is 0.5-2.0%; Mn is 5-8%; Ni is 0.3-2.0%; iron powders are 25-45%; and the total amount of Na2O conversion values and K2O conversion values is 1.5-5.5%.;SELECTED DRAWING: None;COPYRIGHT: (C)2018,JPO&INPIT
机译:解决的问题:提供一种用于低氢型角焊的涂覆焊条,该焊条在确保优异的耐点蚀性的同时,具有低烟尘产生率等优异的焊接加工性,能够获得焊接金属的优异机械性能并且具有良好的焊接性能。解决方案:在用于低氢型角焊的涂层焊条中:相对于涂层剂的总质量,质量百分比为金属碳酸盐的5-15%;金属氟化物的总量为3-8%;金属氟化物中的NaF为0.2-1.5%; TiO 2 的总转化值为5-15%; SiO 2 换算值的总量为10-20%; Al 2 O 3 转换值的总量为0.5-3.0%; FeO转化率的总量为0.5-1.5%; MgO为2-6%; Si为0.5〜2.0%。 Mn为5-8%; Ni为0.3〜2.0%。铁粉为25-45%; Na 2 O转换值和K 2 O转换值的总和为1.5-5.5%.;选定的图纸:无;版权所有:(C)2018,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号