Welding material for ferritic heat resistant steel, welded joint for ferritic heat resistant steel, and method for producing welded joint for ferritic heat resistant steel

机译:铁素体耐热钢的焊接材料,铁素体耐热钢的焊接接头以及生产铁素体耐热钢的焊接接头的方法

摘要

When welding ferritic heat resistant steels containing B, a weld material for ferritic heat resistant steel, weld joint for ferritic heat resistant steel, and weld for ferritic heat resistant steel capable of forming a weld metal having high creep strength and toughness A method for manufacturing a joint is provided. The weld material for ferritic heat resistant steel according to the present embodiment is mass%, C: 0.06 to 0.10%, Si: 0.1 to 0.4%, Mn: 0.3 to 0.7%, Co: 2.6-3.4%, Ni: 0.01-1.10%, Cr: 8.5-9.5%, W: 2.5-3.5%, Nb: 0.02- Contains 0.08%, V: 0.1-0.3%, Ta: 0.02-0.08%, B: 0.007-0.015%, N: 0.005-0.020% The balance is composed of Fe and impurities, and has a chemical composition satisfying the formula (1). 0.5 ≦ Cr + 6Si + 1.5W + 11V + 5Nb + 10B-40C-30N-4Ni-2Co-2Mn ≦ 10.0 (1)
机译:当焊接含有B的铁素体耐热钢时,铁素体耐热钢的焊接材料,铁素体耐热钢的焊接接头以及能够形成具有高蠕变强度和韧性的焊接金属的铁素体耐热钢的焊接方法提供关节。本实施方式的铁素体系耐热钢用焊接材料为质量%,C:0.06〜0.10%,Si:0.1〜0.4%,Mn:0.3〜0.7%,Co:2.6〜3.4%,Ni:0.01〜1.10。 %,Cr:8.5-9.5%,W:2.5-3.5%,Nb:0.02-含0.08%,V:0.1-0.3%,Ta:0.02-0.08%,B:0.007-0.015%,N:0.005-0.020 %余量由Fe和杂质组成,并且具有满足式(1)的化学组成。 0.5≤Cr + 6Si + 1.5W + 11V + 5Nb + 10B-40C-30N-4Ni-2Co-2Mn≤10.0(1)

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号