首页> 外国专利> Method for producing slab for ferritic stainless cold rolled steel sheet and method for manufacturing ferritic stainless cold rolled steel sheet

Method for producing slab for ferritic stainless cold rolled steel sheet and method for manufacturing ferritic stainless cold rolled steel sheet

机译:铁素体不锈钢冷轧板坯的制造方法及铁素体不锈钢冷轧板的制造方法

摘要

PROBLEM TO BE SOLVED: To provide a ferritic stainless cold rolled steel sheet excellent in surface quality and a manufacturing method therefor.SOLUTION: It contains C: 0.002 to 0.020%, N: 0.001 to 0.020%, Si: 0.01 to 2.00%, Mn: 0.01 to 1.00%, P: 0.04% or less, S: 0.02% or less, Al: 0.01 to 0.40%, Cr: 11.5% to 25.0%, Ni: 0.01 to 1.00%, Ti: 0.01 to 0.45% and the balance Fe with inevitable impurities. It is manufactured from a slab after continuous casting with maximum cross section area of a TiN cluster present in a zone in 10 mm from a surface of less than 625 m. A molten steel temperature during casting is set at T(°C)=1559-1.55×Cr% or more or T(°C))=1559-1.55×Cr%+(Ti%×N%-3.5×10)×(3486×Si%+5632) or more by a Ti%×N% value.
机译:解决的问题:提供表面品质优异的铁素体系不锈钢冷轧钢板及其制造方法。解决方案:含有C:0.002〜0.020%,N:0.001〜0.020%,Si:0.01〜2.00%,Mn。 :0.01〜1.00%,P:0.04%以下,S:0.02%以下,Al:0.01〜0.40%,Cr:11.5〜25.0%,Ni:0.01〜1.00%,Ti:0.01〜0.45%平衡铁与不可避免的杂质。它是在连续铸造后由板坯制成的,TiN团簇的最大横截面面积在距小于625 m的表面10mm的区域中。铸造时的钢水温度为T(℃)= 1559-1.55×Cr%以上或T(℃))= 1559-1.55×Cr%+(Ti%×N%-3.5×10)× Ti%×N%的值在(3486×Si%+ 5632)以上。

著录项

  • 公开/公告号JP6306353B2

    专利类型

  • 公开/公告日2018-04-04

    原文格式PDF

  • 申请/专利权人 JFEスチール株式会社;

    申请/专利号JP20140008444

  • 发明设计人 吉野 正崇;太田 裕樹;

    申请日2014-01-21

  • 分类号C22C38;B22D11;B22D11/18;C22C38/50;

  • 国家 JP

  • 入库时间 2022-08-21 13:07:01

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号