Aqueous emulsion, method for producing aqueous emulsion, aqueous pressure-sensitive adhesive composition, and pressure-sensitive adhesive sheet

机译:水性乳液,水性乳液的制造方法,水性压敏胶粘剂组合物和压敏胶粘片

摘要

Step (I) of emulsion polymerization of the first polymerizable component in the presence of an addition-cleavage type chain transfer agent, and a step of supplying the second polymerizable component to the polymer obtained in the step (I) for polymerization. (II) and an aqueous emulsion obtained by the manufacturing method which satisfy | fills the following conditions. The amount of the addition cleavage type chain transfer agent is 0.05 to 1 part by mass with respect to 100 parts by mass of the total polymerizable component obtained by adding the first polymerizable component and the second polymerizable component. A 1st polymeric component gives the polymer whose glass transition temperature is -20 degrees C or less, and is 70-95 mass% in all the polymeric components. A 2nd polymeric component gives the polymer whose glass transition temperature is 50 degreeC or more, and is 5-30 mass% in all the polymeric components.
机译:在加成裂解型链转移剂的存在下,使第一可聚合组分乳液聚合的步骤(I),以及将第二可聚合组分提供给在步骤(I)中获得的用于聚合的聚合物的步骤。 (II)和通过制造方法获得的满足|的水乳液。满足以下条件。相对于100质量份通过添加第一聚合性成分和第二聚合性成分而得到的聚合性成分总量,加成裂解型链转移剂的量为0.05质量份〜1质量份。第1聚合物成分是玻璃化转变温度为-20℃以下,且全部聚合物成分为70〜95质量%的聚合物。第二聚合物成分是玻璃化转变温度为50℃以上且在全部聚合物成分中为5〜30质量%的聚合物。

著录项

  • 公开/公告号JPWO2016194891A1

    专利类型

  • 公开/公告日2018-04-19

    原文格式PDF

  • 申请/专利权人 昭和電工株式会社;

    申请/专利号JP20170521946

  • 发明设计人 奥原 健太;安井 義勝;

    申请日2016-05-31

  • 分类号C08F291;C08F293;C08F2/38;C09J133/04;C09J7/20;

  • 国家 JP

  • 入库时间 2022-08-21 13:06:52