Ferrocene catalyzed method for preparing carbon nanotubes

机译:二茂铁催化制备碳纳米管的方法

摘要

A method for preparing multi-wall carbon nanotubes comprising atomizing a precursor solution comprising an aromatic hydrocarbon and a carrier gas. The mixture is then injected through an ultrasonic atomization system to form atomized precursor droplets. Then by injecting the atomized precursor droplets from the top of a vertical chemical vapor deposition reactor, the droplets can then react with a reaction gas in the reactor vessel to form a film that adsorbs to a growth surface in the reactor vessel. Layer by layer multi-wall carbon nanotubes are formed. This method is repeated to form layers of the multi-wall carbon nanotubes. The nanotubes formed have an outer diameter of 10 nm-51 nm and a length to diameter aspect ratio of 7200-13200.
机译:一种制备多壁碳纳米管的方法,其包括雾化包含芳族烃和载气的前体溶液。然后将混合物通过超声雾化系统注入以形成雾化的前体液滴。然后,通过从垂直化学气相沉积反应器的顶部注入雾化的前体液滴,这些液滴随后可以与反应器容器中的反应气体反应,形成吸附到反应器容器中生长表面的薄膜。形成逐层的多壁碳纳米管。重复该方法以形成多壁碳纳米管的层。形成的纳米管具有10nm-51nm的外径和7200-13200的长径纵横比。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号