An environmental protection cold mixing type modulus-adjustable pavement material and preparation method thereof. Equal components of waterborne epoxy resin and waterborne curing agent are added in a container to obtain a waterborne epoxy resin mixture. Emulsified bitumen, the waterborne epoxy resin mixture, an emulsifying agent, a defoaming agent and a stabilizing agent are prepared according to a certain mass ratio; the emulsified bitumen is first added in the container, and the pH is regulated with hydrochloric acid to be 5.0 to 6.5; the above-mentioned other materials are added and stirred to make mixed liquid; a stator of a high-speed shearing machine is put into the mixed liquid, and the rotational speed is set as 350 to 500 rpm for about 20 to 40 min to obtain waterborne epoxy emulsified bituminous emulsion. B. Coarse aggregate, fine aggregate, fillers, cement and the waterborne epoxy emulsified bitumen obtained from the above-mentioned preparation are selected in proportion; and after the coarse aggregate, the fine aggregate and rubber powder are added in a stirring machine of asphalt mixture and stirred and the waterborne epoxy emulsified bitumen is added and stirred, the cement is added and stirred.
机译:环保型冷拌型模数可调路面材料及其制备方法。将水性环氧树脂和水性固化剂的相同成分添加到容器中,以获得水性环氧树脂混合物。按照一定的质量比制备乳化沥青,水性环氧树脂混合物,乳化剂,消泡剂和稳定剂。首先将乳化沥青加入到容器中,并用盐酸调节pH值至5.0至6.5。加入上述其他材料并搅拌制成混合液。将高速剪切机的定子放入混合液中,并将转速设定为350至500 rpm,持续约20至40分钟,以获得水性环氧乳化沥青乳液。 B.按上述比例选择由上述制备方法得到的粗骨料,细骨料,填料,水泥和水性环氧乳化沥青;粗骨料后,将细骨料和橡胶粉加入沥青混合料的搅拌机中搅拌,并加入水性环氧乳化沥青搅拌,加入水泥搅拌。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号