The invention relates to the building materials industry - for road construction, in the manufacture of concrete and reinforced concrete products or structures, and also mortars. The technical result is the production of a new road surface, as well as construction concrete and reinforced concrete products or structures resistant to external mechanical and thermal impacts, aggressive environments, with increased crack resistance, hydrophobicity and production safety, during which no harmful substances (hydrogen sulphide and sulfurous anhydride) are emitted. The object of the invention is to develop a method for obtaining of FSSC having high resistance to corrosive environments, low and high temperatures, dynamic overloads, and the use in production of a sulfur-concrete mixture of industrial environmental waste for their utilization and elimination of occupational hazards. The said goal is achieved by a certain sequence, consisting of two stages: stage I - production of sulfur binder - modified sulfur (sulfur copolymer) produced from the lump sulfur acid by means of the vortex bed apparatus (VBA) with maximum capacity of 15-35 m/h; stage II - production of FSSC - at a mobile asphalt plant, sulfur binder and organic additives with inert fillers are mixed and heated (temperature no higher than 120°C, for 20-30 minutes): drilling sludge, basalt fiber and construction sand, resulting in melting of the modified sulfur (sulfur copolymer) in the environment of organic additives and inert fillers, for disperse reinforcement and composite.
机译:本发明涉及用于道路建设的建筑材料工业,用于制造混凝土和钢筋混凝土产品或结构,以及砂浆。技术成果是生产新的路面以及耐外部机械和热冲击,侵蚀性环境,抗裂性,疏水性和生产安全性增强的建筑混凝土和钢筋混凝土产品或结构,在此期间,无有害物质(排放出硫化氢和亚硫酸酐)。发明内容本发明的目的是开发一种用于获得FSSC的方法,所述FSSC具有高的耐腐蚀性环境,低温和高温,动态过载,以及在工业环境废物的硫-混凝土混合物的生产中用于其利用和消除的方法。职业危害。所述目标是通过一定的顺序来实现的,该顺序包括两个阶段:第一阶段-硫粘合剂的生产-块状硫酸通过涡流床设备(VBA)产生的改性硫(硫共聚物),最大容量为15 -35 m / h;第二阶段-FSSC的生产-在移动式沥青厂中,将硫磺粘合剂和具有惰性填料的有机添加剂混合并加热(温度不高于120°C,持续20-30分钟):钻探淤渣,玄武岩纤维和建筑砂导致改性的硫(硫共聚物)在有机添加剂和惰性填料的环境中熔融,用于分散增强和复合材料。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号