首页> 外国专利> A METHOD OF SYNTHESIS OF AN ANTI-CORROSION ADDITIVE TO ORGANIC COATING COMPOSITIONS AND AN ORGANIC COATING COMPOSITION WITH AN ANTI-CORROSION ADDITIVE

A METHOD OF SYNTHESIS OF AN ANTI-CORROSION ADDITIVE TO ORGANIC COATING COMPOSITIONS AND AN ORGANIC COATING COMPOSITION WITH AN ANTI-CORROSION ADDITIVE

机译:合成有机涂料组合物的防腐添加剂和具有防腐涂料的有机涂料组合物的方法

摘要

A method of synthesis of an anti-corrosion additive to organic coating compositions, comprising preparing an aqueous reaction solution at a temperature lower than an ambient temperature. The aqueous reaction solution comprises: at least one acid selected from the group consisting of: phosphoric (V) acid, sulfuric (VI) acid, nitric (V) acid, hydrochloric acid, hydrofluoric acid, perchloric acid having a total concentration in aqueous solution from 0,1 to 8 M; at least one oxidant selected from the group consisting of: ammonium persulfate and hydrogen peroxide; aniline in the amount necessary to obtain the weight ratio of aniline:oxidant from 1:2,5 to 1:5; and an anion donor in the amount necessary to obtain the weight ratio of anion donor:aniline not less than 0,1:1. The method comprises, while preparing the aqueous reaction solution, introducing to the aqueous reaction solution: as the anion donor, a compound comprising anions selected from the group consisting of: hexacyanoferrates (III) [Fe(CN)63-] and silicates (SiO32-); at least one compound being iron (III) ion (Fe3+) donor in the amount necessary to obtain the concentration of iron ions (Fe3+) in the reaction mixture in a range from 0,05 to 0,15 M; next, stirring the reaction mixture until the precipitate is precipitated; filtering and drying the precipitate; to obtain a product of the reaction which is a hybrid PANI compound selected from the group consisting of: PANI hexacyanoferrate (III) and PANI silicate.
机译:一种合成有机涂料组合物的防腐添加剂的方法,包括在低于环境温度的温度下制备反应水溶液。反应水溶液包含:在水溶液中具有总浓度的至少一种酸,其选自:磷酸(V)酸,硫酸(VI)酸,硝酸(V)酸,盐酸,氢氟酸,高氯酸从0.1到8 M;至少一种选自过硫酸铵和过氧化氢的氧化剂;获得苯胺:氧化剂的重量比为1∶2.5至1∶5所需的量的苯胺;为了获得阴离子供体:苯胺的重量比不小于0.1∶1所需的量的阴离子供体。该方法包括在制备反应水溶液的同时向反应水溶液中引入:作为阴离子供体的包含选自以下的阴离子的化合物:高铁六氰酸盐(III)[Fe(CN) 6 3-]和硅酸盐(SiO 3 2-);至少一种化合物是获得反应混合物中铁离子(Fe 3 + )浓度所需的量的铁(III)离子(Fe 3 + )供体在0.05至0.15M的范围内;接下来,搅拌反应混合物直至沉淀沉淀。过滤并干燥沉淀物;得到反应产物,该产物是选自以下的杂合PANI化合物:PANI六氰合铁酸酯(III)和PANI硅酸盐。

著录项

  • 公开/公告号WO2018019923A1

    专利类型

  • 公开/公告日2018-02-01

    原文格式PDF

  • 申请/专利权人 NANOPURE SP. Z O.O.;

    申请/专利号WO2017EP68963

  • 发明设计人 SZYMANSKI WOJCIECH;

    申请日2017-07-27

  • 分类号C09D5/08;C08G73/02;

  • 国家 WO