首页> 外国专利> Beneficiation method for high-clay mixed lead-zinc oxide-sulfide ore

Beneficiation method for high-clay mixed lead-zinc oxide-sulfide ore

机译:高黏土氧化铅锌硫化矿混合选矿方法

摘要

#$%^&*AU2017101078B420180524.pdf#####ABSTRACT A beneficiation method for high-clay mixed lead-zinc oxide-sulfide ore including the steps of: a. performing ore crushing and/or ball milling of a raw mixed lead-zinc oxide5 sulfide ore to provide a ground ore where 75% or more of the ground ore has a particle size of less than 0.074mm; b. passing the ground ore to an agitator barrel, and carrying out froth flotation to produce a lead concentrate and lead deficient stream; c. passing the lead deficient stream to a zinc sulphide flotation step to obtain 10 a zinc sulfide concentrate and a zinc sulphide deficient stream; d. dewatering and optionally desliming, the zinc sulphide deficient stream and then performing a slurry mixing in a thick pulp procedure by the addition of water and chemical additives to enhance sulfatization on the surface of the zinc oxide ore in the zinc sulphide deficient stream and 15 e. performing froth flotation on the dewatered zinc sulphide deficient stream to obtain a zinc oxide concentrate. The beneficiation method for high-clay mixed lead-zinc oxide-sulfide ore not only enhances the grades of lead and zinc concentrates, but also during beneficiation, reagents and tailings water can be recycled, thereby reducing environmental pollution. 20
机译:#$%^&* AU2017101078B420180524.pdf #####抽象一种高黏土混合氧化锌铅锌矿的选矿方法,包括步骤:一种。对原始的混合铅锌氧化物进行矿石破碎和/或球磨5硫化矿石可提供地面矿石,其中75%或更多的地面矿石具有颗粒尺寸小于0.074mm;b。将地面矿石送至搅拌桶,并进行泡沫浮选产生铅精矿和铅缺乏物流;C。将缺乏铅的料流进行硫化锌浮选步骤以得到10硫化锌精矿和缺乏硫化锌的料流;d。对缺乏硫化锌的物流进行脱水和除泥然后通过添加水以浓浆程序进行浆液混合和化学添加剂以增强氧化锌矿石表面的硫酸化硫化锌缺乏物流和15日在脱水的硫化锌不足物流上进行泡沫浮选得到氧化锌浓缩物。高粘土混合氧化铅锌锌矿的选矿方法提高了铅和锌精矿的品位,而且在选矿过程中,试剂和尾矿水可以循环使用,从而减少环境污染。20

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号