SOUR-RESISTANT HEAVY-WALLED STEEL MATERIAL HAVING EXCELLENT LOW-TEMPERATURE TOUGHNESS AND POST-HEAT TREATMENT CHARACTERISTICS AND METHOD FOR MANUFACTURING SAME

机译:具有出色的低温韧性和后热处理特性的耐酸重钢材料及其制造方法

摘要

Provided are: a SOUR-resistant heavy-walled steel material having excellent low-temperature toughness and post-heat treatment characteristics; and a method for manufacturing the same. The SOUR-resistant heavy-walled steel material of the present invention comprises: in terms of weight%, 0.02-0.06% of C; 0.5% or less of Si (excluding 0%); 0.8-2.0% of Mn; 0.03% or less of P; 0.003% or less of S; 0.06% or less of Al; 0.01% or less of N; 0.005-0.1% of Nb; 0.005-0.05% of Ti; 0.0005-0.005% of Ca; one or more selected from 0.05-0.5% of Ni, 0.05-0.5% of Cr, 0.02-0.4% of Mo, and 0.005-0.1% of V; and the remainder Fe and unavoidable impurities, wherein the heavy-walled steel material satisfies relational expressions 1-3, and has a percent ductile fracture of 85% or more in the drop weight tear test (DWTT) at -20°C.
机译:提供:具有优异的低温韧性和后热处理特性的耐酸的厚壁钢材;及其制造方法。本发明的耐SOUR的重壁钢材包含:以重量%计,C为0.02〜0.06%。 0.5%以下的Si(0%除外); Mn 0.8-2.0%; P的0.03%以下; S的0.003%以下; Al的0.06%以下; N的0.01%以下Nb的0.005-0.1%; Ti的0.005-0.05%;钙0.0005-0.005%; Ni中的0.05-0.5%,Cr的0.05-0.5%,Mo的0.02-0.4%和V的0.005-0.1%中的一种或多种;其余的铁和不可避免的杂质,其中,该厚壁钢材满足关系式1-3,并且在-20℃下的落锤撕裂试验(DWTT)中具有85%以上的延性断裂百分数。

著录项

  • 公开/公告号WO2018117450A1

    专利类型

  • 公开/公告日2018-06-28

    原文格式PDF

  • 申请/专利权人 POSCO;

    申请/专利号WO2017KR13553

  • 发明设计人 KOH SEONG-UNG;PARK JAE-HYUN;BAE MOO-JONG;

    申请日2017-11-24

  • 分类号C22C38/44;C22C38/46;C22C38;C22C38/58;C22C38/02;C22C38/06;C21D9/46;C22C38/48;C22C38/50;C21D8/02;

  • 国家 WO

  • 入库时间 2022-08-21 12:43:39

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号