首页> 外国专利> METHOD FOR PREPARING RICE EAR-SHAPED COPPER PARTICLES, RICE EAR-SHAPED COPPER PARTICLES PREPARED THEREBY, AND CONDUCTIVE PASTE USING SAME

METHOD FOR PREPARING RICE EAR-SHAPED COPPER PARTICLES, RICE EAR-SHAPED COPPER PARTICLES PREPARED THEREBY, AND CONDUCTIVE PASTE USING SAME

机译:制备米耳形铜颗粒的方法,由此制备的米耳形铜颗粒和使用相同的导电糊

摘要

The present invention relates to rice ear-shaped copper particles, and the subject matter are: a method for preparing rice ear-shaped copper particles; rice ear-shaped copper particles prepared thereby; and a conductive paste using the same, the method comprising: a first step of preparing a copper precursor solution; a second step of adjusting the pH of the copper precursor solution; a third step of adding a zinc powder to the pH-adjusted copper precursor solution; a fourth step of synthesizing rice ear-shaped copper particles by stirring the copper precursor solution, to which zinc powder was added, for a predetermined time; and a fifth step of separating, washing, and then drying the synthesized rice ear-shaped copper particles.
机译:稻穗状铜粒子的制造方法技术领域本发明涉及稻穗状铜粒子的制造方法。由此制得的稻穗形铜颗粒;该方法包括:制备铜前驱体溶液的第一步;调节铜前体溶液的pH的第二步骤;第三步,将锌粉加入到pH调节的铜前体溶液中;第四步骤是通过搅拌添加有锌粉的铜前驱体溶液预定时间来合成米穗形铜颗粒。第五步,分离,洗涤,然后干燥合成的稻穗形铜颗粒。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号