The present invention provides a concrete crack recovery performance test method, comprising the steps of: applying a cylinder-shaped concrete test piece by using epoxy as a whole; dividing the applied concrete test piece into two halves; disposing the bisected concrete test piece between an aqueous 5%-NaCl solution and an aqueous 0.3 N-NaOH solution; measuring chlorine ions passing through the bisected concrete test piece by applying DC voltage of 40 V to 80 V to the aqueous 5%-NaCl solution and the aqueous 0.3 N-NaOH solution for 4 to 8 hours; providing non-hydrated C_2S or non-hydrated C_3S and moisture to the cracked surface of the bisected concrete test piece so as to heal cracks; disposing the crack-healed concrete test piece between an aqueous 5%-NaCl solution and an aqueous 0.3 N-NaOH solution; and measuring chlorine ions passing through the crack-healed concrete test piece by applying DC voltage of 40 V to 80 V to the aqueous 5%-NaCl solution and the aqueous 0.3 N-NaOH solution for 4 to 8 hours.;COPYRIGHT KIPO 2018
机译:本发明提供了一种混凝土裂缝恢复性能测试方法,包括以下步骤:整体上使用环氧树脂涂覆圆筒形混凝土测试件;将涂覆的混凝土试件分为两半;将等分的混凝土试件放置在5%NaCl水溶液和0.3 N-NaOH水溶液之间;通过在5%-NaCl水溶液和0.3N-NaOH水溶液中施加40 V至80 V的直流电压4至8小时,测量通过等分混凝土试件的氯离子。向平分的混凝土试件的破裂表面提供非水合的C_2S或非水合的C_3S和水分,以修复裂缝。将裂缝愈合的混凝土试件放置在5%NaCl水溶液和0.3 N-NaOH水溶液之间;通过在5%-NaCl水溶液和0.3N-NaOH水溶液中施加40 V至80 V的直流电压4至8小时来测量通过裂缝愈合的混凝土试件的氯离子。; COPYRIGHT KIPO 2018

著录项

  • 公开/公告号KR20180060535A

    专利类型

  • 公开/公告日2018-06-07

    原文格式PDF

  • 申请/专利权人 JACE KOREA. INC.;

    申请/专利号KR20160160109

  • 发明设计人 LEE SANG CHULKR;

    申请日2016-11-29

  • 分类号G01N27/04;C04B41/45;G01N1/28;G01N33/38;

  • 国家 KR

  • 入库时间 2022-08-21 12:39:55

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号