METHOD OF ARC WELDING OF TRIPLE CONNECTIONS (WELDOLETS) OF THE MAIN PIPELINES

机译:主管道三重连接(焊接)的电弧焊接方法

摘要

FIELD: electricity.;SUBSTANCE: technological hole in the pipe is made. Welding groove is performed, edges in the temperature range from 150 to 200°C are pre-heated and intermediate layer of welded metal is applied to the weldolet grooving surface with thickness from 4 to 7 mm. Then, the welded rollers are applied over the contour of the grooving with the formation of a welded belt with a width of at least 2.5 of the pipe wall thickness and cooling the welded joint by applying a heat-insulating belt. Wherein, when this intermediate layer is applied, metal is used, mechanical properties, of which according to the criterion of elongation are on 18-35% higher than mechanical properties according to the criterion of the elongation of the parent pipe metal and welded layers of weld metal. The superposition of welding rolls is carried out with the exposure of interlayer temperature between the superposed welding rollers in the temperature range from 50 to 250°C.;EFFECT: invention allows to improve the quality of welded joint.;5 cl, 1 tbl, 1 ex
机译:领域:电力;实体:在管道中制造工艺孔。执行焊接凹槽,将温度范围从150到200°C的边缘预热,并将焊接金属的中间层应用到厚度为4到7毫米的weltolet开槽表面。然后,将焊接辊施加到开槽轮廓上,形成宽度至少为管壁厚度2.5的焊接带,并通过应用隔热带冷却焊接接头。其中,当使用该中间层时,使用金属,其机械性能根据伸长率的标准比根据母管金属和焊接层的伸长率的机械性能高18-35%。焊接金属。堆焊辊的叠置是在暴露的堆焊辊之间的层间温度在50至250°C的温度范围内进行的。效果:本发明可以提高焊接接头的质量。5cl,1 tbl, 1前

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号