FIELD: electricity.;SUBSTANCE: pressed metal-alloy palladium-barium cathode is made of a three-layer of two continuous palladium ribbons and a ribbon placed between them with spaced holes at equal distances forming the cells with powder of intermetallide Pd5Ba. The method for producing the noted cathode involves the preparation of a powder of intermetallide Pd5Ba by melting the intermetallide Pd5Ba, its grinding in an atmosphere of inert gases or CO2. A palladium ribbon is covered with the palladium ribbon made with equiparticular holes spaced at equal distances, Pd5Ba intermetallide powder is poured into the holes of the palladium ribbon, palladium ribbon, the same as the lower one, with the through holes is placed on top of the palladium ribbon, the resulting three-layer structure is pressed under pressure 10-12 t/cm2, after which it is annealed for 1-2 hours in an inert atmosphere at a temperature of 800-900 °C and hot rolling is carried out to a given thickness.;EFFECT: increase in the coefficient of secondary electron emission.;2 cl, 2 dwg, 2 tbl, 2 ex
机译:领域:电力。物质:压制金属钯钯阴极是由三层连续的两个钯带和一个位于带之间的带组成,带之间等距间隔开有金属间内化物Pd 粉末形成的电池5 Ba制备所述阴极的方法包括通过熔化金属间化合物Pd 5 Ba制备金属间化合物Pd 5 Ba粉末,在惰性气体或CO气氛中对其进行研磨。 2 。钯带上覆盖有等间距等距离间隔开的钯带,将Pd 5 Ba金属间化合物粉末倒入钯带的孔中,钯带与下部的孔相同,将通孔置于钯带的顶部,在10-12 t / cm 2 的压力下对所得的三层结构进行压制,然后在真空中退火1-2小时。惰性气氛,在800-900°C的温度下进行热轧至给定的厚度;效果:二次电子发射系数的增加; 2 cl,2 dwg,2 tbl,2 ex

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号