METHOD OF PROCESSING OF CONTACTING SEALING SURFACES ELEMENTS MADE FROM HEAT-RESISTANT ALLOYS OF THE PULSE FACE SEAL (PFS) OPERATING IN CRYOGENIC ENVIRONMENTS (VARIANTS)

机译:在低温环境(变体)中操作的脉冲面密封(PFS)的耐热合金制成的接触密封表面元素的处理方法

摘要

FIELD: molding.;SUBSTANCE: invention relates to the field of electrophysical and electrochemical machining, in particular to electroerosive alloying, and can be used for surfaces treatment of the impulse end seals elements. First variant of the method includes electroerosive alloying of the contacting surfaces made from the heat-resistant alloy HN58MBUD graphite electrode in front of which an electroerosive coating of copper or nickel is applied to contact surface at a discharge energy Wu = 0.04 J and Wu = 0.03 J, respectively, and to the other contact surface an electroerosive coating of copper is applied at a discharge energy of Wu = 0.02 J, besides the doping with a graphite electrode is performed at a discharge energy of Wu = 0.05-0.2 J. Second variant of the method includes electroerosive alloying of the contacting surfaces from beryllium bronze BrB2 with a graphite electrode in front of which an electroerosive coating of copper is applied to one of the contacting surfaces at a discharge energy of Wu = 0.08 J, wherein the doping with a graphite electrode is performed at a discharge energy of Wu = 0.05-0.2 J.;EFFECT: invention provides a reduction in microhardness and an increase in ductility of the contacting sealing surfaces of the pulse mechanical seal elements to reduce the contact pressure and increase the tightness of the joint.;2 cl, 1 tbl
机译:脉冲端密封件的表面处理技术领域本发明涉及电物理和电化学加工领域,尤其涉及电腐蚀合金,并且可用于脉冲端密封件的表面处理。该方法的第一个变体包括对由耐热合金HN58MBUD石墨电极制成的接触面进行电腐蚀合金化,在其前面以放电能量Wu = 0.04 J和Wu = 0.03将铜或镍的电腐蚀涂层施加到接触表面分别在J和另一接触表面上以Wu = 0.02 J的放电能量施加铜的电腐蚀涂层,除了在Wu = 0.05-0.2 J的放电能量下进行石墨电极掺杂之外。该方法的一种方法包括将铍青铜BrB2与石墨电极的接触表面进行电腐蚀合金化,在石墨电极的前面将铜的电腐蚀涂层以Wu = 0.08 J的放电能量施加到其中一个接触表面上,其中掺杂有石墨电极的放电能量为Wu = 0.05-0.2 J。;效果:本发明提供了显微硬度的降低和c的延展性的提高脉冲机械密封元件的完整密封表面可降低接触压力并提高接头的紧密度。; 2 cl,1 tbl

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号