FIELD: technological processes.;SUBSTANCE: invention relates to the production of wear-resistant coatings and can be used to expand the range of machine parts and tools. Method for producing a wear-resistant gradient coating of the Ti-Al system on a steel part in a vacuum includes depositing an intermetallic compound coating of the Ti-Al system from a vacuum arc discharge plasma for 180 minutes at a pressure of 1.5*10-1 Pa in an inert gas in the form of argon and currents of arc evaporators in the range of 60–120 A and subsequent nitriding in an arc discharge by means of a plasma source with an incandescent cathode for 60 min at a pressure of 2*10-1 Pa in a reaction gas in the form of nitrogen, the current of a incandescent cathode 100 A, and the current of an arc discharge of the plasma source 50 A and the temperature of the part 550 °C.;EFFECT: provides the wear-resistant gradient coating, increasing the mechanical properties and adhesion strength of the coating.;1 cl, 5 dwg, 1 tbl, 1 ex
机译:技术领域;技术领域;本发明涉及耐磨涂层的生产,并且可以用于扩大机械零件和工具的范围。在真空中在钢部件上产生Ti-Al系统的耐磨梯度涂层的方法包括:在1.5 * 10的压力下,从真空电弧放电等离子体中沉积Ti-Al系统的金属间化合物涂层180分钟。 -1 Pa在氩气形式的惰性气体中以及60-120 A范围内的电弧蒸发器电流,随后通过带有白炽阴极的等离子源在电弧放电中氮化在氮气形式的反应气体,白炽阴极100 A的电流和等离子源50的电弧放电的电流中,在2 * 10 -1 Pa压力下60分钟A和零件温度550°C .;效果:提供耐磨的梯度涂层,提高涂层的机械性能和粘合强度。; 1 cl,5 dwg,1 tbl,1 ex

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号