首页> 外国专利> Complex halogen-free solid flame retardant composition, process for its preparation and polymer molding compositions and their use

Complex halogen-free solid flame retardant composition, process for its preparation and polymer molding compositions and their use

机译:复合无卤固体阻燃剂组合物,其制备方法和聚合物模塑组合物及其用途

摘要

Complex halogen-free solid flame retardant composition for polymer molding compositions consisting of 30 to 70 wt .-% porous, low-melting glass particles from a high temperature extruded borosilicate glass foam having an average particle size of 1.5 to 12 .mu.m 30 to 70 wt .-% melamine and - 2 to 10 wt .-% ammonium nitrate, which by-dry mixing of the porous glass particles of a borosilicate glass foam and the melamine uniform distribution of 2-10 wt .-% ammonium nitrate dissolved in distilled water, in the mixture of the glass particles and the Melamine further mixing the components porous glass particles, melamine and dissolved ammonium nitrate temperature treatment of the mixture at 90 to 120 ° C for 90 to 240 minutes.
机译:用于聚合物模塑组合物的复合无卤固体阻燃剂组合物,由来自高温挤出的硼硅酸盐玻璃泡沫的30至70 wt。%的多孔低熔点玻璃颗粒组成,平均粒径为1.5至12μm30 -70重量%的三聚氰胺和-2-10重量%的硝酸铵,它们通过干燥混合硼硅酸盐玻璃泡沫的多孔玻璃颗粒和3-10重量%的溶解的三聚氰胺而均匀分布在蒸馏水中,在玻璃颗粒和三聚氰胺的混合物中进一步混合多孔玻璃颗粒,三聚氰胺和溶解的硝酸铵成分,将混合物在90至120°C温度下处理90至240分钟。

著录项

  • 公开/公告号DE102015015710B4

    专利类型

  • 公开/公告日2018-07-26

    原文格式PDF

  • 申请/专利权人 TROVOTECH GMBH;

    申请/专利号DE20151015710

  • 发明设计人 HANS-JÜRGEN VOSS;

    申请日2015-12-07

  • 分类号C09K21/14;C08L67;C08L77;C09K21/02;C09K21/10;

  • 国家 DE

  • 入库时间 2022-08-21 12:35:00