A glass composition for producing chemically strengthened alkali-aluminosilicate glass and a method for manufacturing the chemically strengthened alkali-aluminosilicate glass. The chemically strengthened alkali-aluminosilicate glass is suitable for use as high-strength cover glass for touch displays, solar cell cover glass and laminated safety glass, and is produced in a shorter amount of time.
机译:用于生产化学强化碱金属铝硅酸盐玻璃的玻璃组合物和用于制造化学强化碱金属铝硅酸盐玻璃的方法。化学强化的碱金属铝硅酸盐玻璃适合用作触摸显示器的高强度防护玻璃,太阳能电池防护玻璃和夹层安全玻璃,并且生产时间较短。

著录项

  • 公开/公告号EP3341333A4

    专利类型

  • 公开/公告日2019-04-24

    原文格式PDF

  • 申请/专利权人 KORNERSTONE MATERIALS TECHNOLOGY CO. LTD;

    申请/专利号EP20150901991

  • 发明设计人 DING YUANJIE;CHEN YIJUN;

    申请日2015-08-26

  • 分类号C03C3/091;C03C4/18;C03C21;C03B17/06;C03B18/02;C03B25/02;

  • 国家 EP

  • 入库时间 2022-08-21 12:29:13

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号