The present invention discloses a method for preparing high-performance tread rubber through a filler silylation reaction catalyzed in situ by an ionic liquid. The method is as follow: adding a gum rubber, a filler, a silane and an ionic liquid successively into an open mill or an internal mixer for mixing to obtain a rubber compound; high-temperature remilling the rubber compound; adding a vulcanizing package and an anti-aging agent into the remilled rubber compound at room temperature; and vulcanizing the rubber compound to obtain a vulcanized rubber. The method uses the ionic liquid as a catalyst for the silylation of filler surfaces, which effectively promotes the dispersion of a light-colored filler such as silica in the rubber, and improves the rubber-filler interfacial performance. Therefore, this method can substantially reduce an amount of the silane and improve dynamic mechanical performance of a tread rubber material, including reduced rolling resistance and heat build-up. This method has advantages such as simple technology and no additional processing equipment or step is needed, having an important prospect in preparation of the high-performance tire.
机译:本发明公开了一种通过离子液体原位催化的填料甲硅烷基化反应制备高性能胎面胶的方法。该方法如下:将胶基橡胶,填充剂,硅烷和离子液体依次加入到开炼机或内部混合器中进行混合以获得橡胶混合物。高温复磨橡胶混合物;在室温下将硫化包和抗老化剂添加到经碾磨的橡胶混合物中;硫化所述橡胶混合物以获得硫化橡胶。该方法使用离子液体作为用于填料表面的甲硅烷基化的催化剂,其有效地促进了浅色填料例如二氧化硅在橡胶中的分散,并改善了橡胶-填料的界面性能。因此,该方法可实质上减少硅烷的量并改善胎面橡胶材料的动态机械性能,包括降低的滚动阻力和热量积聚。该方法具有技术简单,无需额外的加工设备或步骤等优点,在制备高性能轮胎方面具有重要的前景。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号