Thermoplastic compositions include a polycarbonate-siloxane copolymer comprising: from about 49.5 wt % to about 97.95 wt % of at least one polycarbonate polymer; from about 2.0 wt % to about 49.5 wt % of at least one polycarbonate-siloxane r copolymer; and from about 0.05 wt % to about 1.0 wt % of at least one release agent. The composition exhibits a melt volume flow rate of at least about 25 cm3/10 min, a ductile/brittle transition temperature of less than or equal to 10° C., and high gloss after metallization and/or a substantial tensile yield strength retention improvement when exposed to sunscreen. Methods of forming an article include: forming a mixture comprising the thermoplastic composition, and injection molding, extruding, rotational molding, blow molding or thermoforming the mixture in a mold to form the article. Such compositions and methods may be used to form articles including, but not limited to, automotive bezels and housings in consumer devices.
机译:热塑性组合物包括聚碳酸酯-硅氧烷共聚物,其包含:约49.5重量%至约97.95重量%的至少一种聚碳酸酯聚合物;和从约2.0wt%至约49.5wt%的至少一种聚碳酸酯-硅氧烷r共聚物;和约0.05重量%至约1.0重量%的至少一种脱模剂。该组合物表现出至少约25cm 3 / 10min的熔体体积流速,小于或等于10℃的延性/脆性转变温度,以及金属化后的高光泽度和/或显着的拉伸屈服强度保持性改善。当暴露在防晒霜下。形成制品的方法包括:形成包含热塑性组合物的混合物,以及在模具中将混合物注塑,挤出,旋转模塑,吹塑或热成型以形成制品。这样的组合物和方法可以用于形成制品,包括但不限于消费设备中的汽车边框和外壳。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号