This invention relates to the porous ultra-soft ultra-fine denier polyester fiber and its preparation method. The modified polyester is spun with a porous spinneret to produce the porous ultra-soft ultra-fine denier polyester fiber, and the arrangement of the spinneret holes on the porous spinneret is arranged in an elliptical arrangement. That is, the spinning hole center of the spinneret is located on the concentric ellipse, the concentric ellipse is a series of ellipses, all the ellipses are long axis collinear, and short axis collinear. The porous ultra-soft ultra-fine denier polyester fiber is obtained by metering, extruding, cooling, oiling and high-speed winding the modified polyester chips. The preparation method of modified polyester is as follows: terephthalic acid reacts with ethylene glycol to produce ethylene terephthalate. The modified polyester is obtained by the reaction of terephthalic acid with branched diol. The fiber of the invention has good properties and the deviation rate of fiber density. The deviation rate of fiber density is ≤ 0.5%, the CV value of breaking strength is ≤ 4.0%, the CV value of elongation at break is ≤ 8.0%, the CV value of yarn unevenness is≤ 2.0%.
机译:本发明涉及一种多孔超软超细旦聚酯纤维及其制备方法。将改性聚酯用多孔喷丝头纺丝以生产多孔超软超细旦尼尔聚酯纤维,并且在多孔喷丝头上的喷丝孔的布置以椭圆形布置。即,喷丝头的纺丝孔中心位于同心椭圆上,同心椭圆是一系列的椭圆,所有的椭圆都是长轴共线,短轴共线。多孔超软超细旦尼尔聚酯纤维是通过计量,挤出,冷却,上油和高速缠绕改性聚酯切片得到的。改性聚酯的制备方法如下:对苯二甲酸与乙二醇反应生成对苯二甲酸乙二酯。改性聚酯是通过对苯二甲酸与支链二醇反应获得的。本发明的纤维具有良好的性能和纤维密度的偏差率。纤维密度的偏差率≤0.5%,断裂强度的CV值≤4.0%,断裂伸长率的CV值≤8.0%,纱线不匀度的CV值≤2.0%。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号