PROBLEM TO BE SOLVED: To provide a high-strength cement mortar composition having high compressive strength without requiring a large-scale and special manufacturing facility.SOLUTION: A high-strength cement mortar composition comprises cement, silica fume, water, a fine aggregate, a water reducing agent, an antifoaming agent, and a metal fine powder. The cement contains 10.0-40.0 mass% of CS and 40.0-70.0 mass% of CS, and the fine aggregate comprises ferronickel slag. A method for producing hardened high-strength cement mortar includes: a pre-curing step of curing the high-strength cement mortar composition in air at 15-25°C for 1-5 days; a first curing step of curing the high-strength cement mortar composition in water at 20-60°C for 1-7 days; a second curing step of curing the high-strength cement mortar composition in water at 80-100°C for 5-21 days; and a third curing step of curing the high-strength cement mortar composition in air at 80-200°C for 5-21 days.
机译:要解决的问题:提供具有高抗压强度的高强度水泥砂浆组合物,而无需大规模的特殊制造设施。解决方案:高强度水泥砂浆组合物包含水泥,硅粉,水,细骨料,减水剂,消泡剂和金属细粉。水泥包含10.0-40.0质量%的CS和40.0-70.0质量%的CS,细骨料包括镍铁渣。一种硬化的高强度水泥砂浆的生产方法,其包括:预固化步骤,将高强度水泥砂浆组合物在空气中于15-25℃下固化1-5天。第一固化步骤是将高强度水泥砂浆组合物在20-60℃的水中固化1-7天;第二固化步骤是将高强度水泥砂浆组合物在80-100℃的水中固化5-21天。第三固化步骤是将高强度水泥砂浆组合物在80-200℃的空气中固化5-21天。

著录项

  • 公开/公告号JP6530890B2

    专利类型

  • 公开/公告日2019-06-12

    原文格式PDF

  • 申请/专利权人 宇部興産株式会社;

    申请/专利号JP20140060162

  • 发明设计人 桐山 宏和;佐藤 喜英;玉滝 浩司;

    申请日2014-03-24

  • 分类号C04B28/02;C04B7/02;C04B18/14;C04B22/04;C04B24/26;C04B40/02;

  • 国家 JP

  • 入库时间 2022-08-21 12:21:38

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号