Fe-Ni-Cr-Mo合金およびその製造方法

机译:Fe-Ni-Cr-Mo合金及其制造方法

摘要

PROBLEM TO BE SOLVED: To propose an Fe-Ni-Cr-Mo alloy having excellent corrosion resistance and strength when receiving a thermal effect and a method for producing the Fe-Ni-Cr-Mo alloy.;SOLUTION: An Fe-Ni-Cr-Mo alloy contains, in mass%, C: 0.005-0.03%, Si: 0.02-0.70%, Mn: 0.01-1.50%, P: 0.010-0.050%, S: 0.002% or less, Ni: 30.0-32.0%, Cr: 26.0-28.0%, Mo: 3.0-4.0%, N: 0.01-0.10%, Al: 0.015-0.20%, and further contains Cu: 0.7-1.4% and/or Co: 0.003-0.30% with the balance being Fe and inevitable impurities, satisfying the following (1), (2) formulae. 0.8≤[%Cu]+15×[%Co]≤5.5 (1). 2.1≤100×[%Al]+66.7×[%N]≤22.7 (2). There is also provided a method for producing the alloy that includes annealing a hot-rolled steel plate or cold-rolled steel plate produced by conventional methods at 1100-1190°C.;SELECTED DRAWING: Figure 1;COPYRIGHT: (C)2019,JPO&INPIT
机译:要解决的问题:提出一种在受热作用时具有优异的耐腐蚀性和强度的Fe-Ni-Cr-Mo合金以及一种生产Fe-Ni-Cr-Mo合金的方法。 Cr-Mo合金以质量%含有C:0.005-0.03%,Si:0.02-0.70%,Mn:0.01-1.50%,P:0.010-0.050%,S:0.002%以下,Ni:30.0-32.0 %,Cr:26.0-28.0%,Mo:3.0-4.0%,N:0.01-0.10%,Al:0.015-0.20%,并且进一步包含Cu:0.7-1.4%和/或Co:0.003-0.30%,且余量为Fe和不可避免的杂质,满足下式(1),(2)。 0.8≤[%Cu] + 15×[%Co]≤5.5(1)。 2.1≤100×[%Al] + 66.7×[%N]≤22.7(2)。还提供了一种合金的制造方法,该方法包括在1100-1190°C下对通过常规方法制得的热轧钢板或冷轧钢板进行退火;图1;版权:(C)2019,日本特许厅

著录项

  • 公开/公告号JP2019035122A

    专利类型

  • 公开/公告日2019-03-07

    原文格式PDF

  • 申请/专利权人 NIPPON YAKIN KOGYO CO LTD;

    申请/专利号JP20170157529

  • 发明设计人 矢部 室恒;

    申请日2017-08-17

  • 分类号C22C38/00;C22C38/52;C21D8/02;C22C30/02;C21D9/46;

  • 国家 JP

  • 入库时间 2022-08-21 12:20:16

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号