Organoguanidine-nontoxic alcohol catalyzed active lactide ring-opening polymerization controlled process to synthesize polylactic acid

机译:有机胍-无毒醇催化的丙交酯活性开环聚合控制方法合成聚乳酸

摘要

A method for synthesizing polylactide (PLA). The method employs RCOOCG, a nontoxic carboxylate of cyclic guanidine (CG), as a catalyst and non-toxic organic alcohol R′OH as an initiator to catalyze/initiate a living ring-opening polymerization of lactide (LA). The method includes: 1) adding monomer LA, the catalyst RCOOCG, and the initiator R′OH to a reaction still, where an initial molar ratio of the monomer to the catalyst is [LA]0/[RCOOCG]0=1000-1500:1, an initial molar amount [R′OH]0 of the initiator R′OH is determined by a number average molecular weight (Mn) of a target product PLA; 2) removing air in the reaction still, sealing the reaction still after a pressure in the reaction still is constant at between 1.0 and 0.1 torr; stirring and heating the reaction still in 30 to 40 minutes to a temperature between 95 and 96° C.; and allowing reactants in the reaction still to polymerization.
机译:一种合成聚丙交酯(PLA)的方法。该方法使用RCOOCG(一种无毒的环状胍(CG)羧酸盐)作为催化剂,并使用无毒的有机醇R'OH作为引发剂来催化/引发丙交酯(LA)的活性开环聚合。该方法包括:1)在反应釜中加入单体LA,催化剂RCOOCG和引发剂R'OH,其中单体与催化剂的初始摩尔比为[LA] 0 / [RCOOCG] 0 = 1000-1500 1:1,引发剂R'OH的初始摩尔量[R'OH] 0由目标产物PLA的数均分子量(Mn)决定; 2)除去反应釜中的空气,在反应釜中的压力恒定在1.0至0.1托之间之后,将反应釜密封。在30至40分钟内搅拌并加热反应至95至96℃之间的温度;使反应中的反应物仍然聚合。

著录项

  • 公开/公告号JP6538876B2

    专利类型

  • 公开/公告日2019-07-03

    原文格式PDF

  • 申请/专利权人 南京大学;

    申请/专利号JP20170554893

  • 申请日2016-03-22

  • 分类号C08G63/82;C08G63/08;

  • 国家 JP

  • 入库时间 2022-08-21 12:19:55