PROBLEM TO BE SOLVED: To provide an aluminum alloy sheet for an automobile body panel excellent in filiform rust resistance and recycling property and a manufacturing method therefor, an automobile body panel using the same and a manufacturing method therefor.SOLUTION: An aluminum alloy sheet for an automobile body panel excellent in filiform rust resistance and recycling property, is made of an Al alloy containing Mg:0.30 to 0.80 mass% (hereafter referred to as "%"), Si:0.80 to 1.40%, Mn:0.20 to 0.65%, Zn:0.44 to 0.60%, Fe:0.25 to 0.40% and Cu:0.17 to 0.25%, has elongation of 23% at 100 days after solution heat treatment, bearing force after conducting coating galling treatment of 200 MPa or more and further point number in a Heming test based on JISH7701 of 0 to 2 point. The present invention also provides a manufacturing method for the aluminum alloy sheet, an automobile body panel using the aluminum alloy sheet and a manufacturing method therefor.SELECTED DRAWING: None
机译:要解决的问题:提供一种具有优异的丝状耐锈性和再循环特性的用于汽车车身板的铝合金板及其制造方法,使用该铝合金板的汽车板及其制造方法。丝状耐锈性和再利用性优异的汽车车身板由含有Mg:0.30〜0.80质量%(以下称为“%”),Si:0.80〜1.40%,Mn:0.20〜0.65%的Al合金构成。 ,Zn:0.44〜0.60%,Fe:0.25〜0.40%,Cu:0.17〜0.25%,固溶化热处理100天后的伸长率为23%,进行200MPa以上的涂层磨损处理后的承受力。在基于JISH7701的Heming测试中的0到2分。本发明还提供了该铝合金片的制造方法,使用该铝合金片的车身板及其制造方法。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号