A stainless steel plate having excellent corrosion resistance, low contact resistance, and excellent press workability without using expensive raw materials such as gold and rare metals, and a method for producing the same are provided. The method for producing a stainless steel sheet includes a step of preparing a slab having a chemical composition of mass%, including Cr: 20 to 26%, N: 0.1% or less, Si: 2.0% or less, etc. (Step S1) The step of obtaining a rolled steel sheet having a thickness of 50 to 200 μm by hot-rolling and cold-rolling the slab (step S2), and the annealing process of annealing and cooling the rolled steel sheet in a gas atmosphere containing nitrogen. (Step S3) and a step (Step S4) of pickling the rolled steel sheet after the annealing step with a solution containing a non-oxidizing acid. The stainless steel plate has an N content of 0.6 to 2.0 mass%.
机译:本发明提供一种不使用金,稀有金属等昂贵的原料而具有优异的耐腐蚀性,低接触电阻和优异的冲压加工性的不锈钢板及其制造方法。该不锈钢板的制造方法包括以下步骤:制备具有质量%的化学成分的板坯,所述化学成分包括Cr:20〜26%,N:0.1%以下,Si:2.0%以下等(步骤S1)。 )通过对板坯进行热轧和冷轧而获得厚度为50至200μm的轧制钢板的步骤(步骤S2),以及在含氮的气体气氛中对轧制钢板进行退火和冷却的退火工艺。 。 (步骤S3)和退火步骤后的轧制钢板用包含非氧化性酸的溶液酸洗的步骤(步骤S4)。不锈钢板的N含量为0.6〜2.0质量%。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号