Method for suppressing rear face oxidation of carbon-containing refractory, lining structure, and carbon-containing refractory

机译:抑制含碳耐火材料,衬里结构和含碳耐火材料的背面氧化的方法

摘要

Provided is a method for suppressing rear face oxidation and a lining structure, with which high airtightness and a great effect of suppressing rear face oxidation are obtained. The method for suppressing rear face oxidation of a carbon-containing refractory includes forming an adherent layer on a rear face of a carbon-containing refractory by applying an alkali metal silicate aqueous solution to the rear face and solidifying the alkali metal silicate aqueous solution. The alkali metal silicate aqueous solution contains an alkali metal oxide R2O (R is an alkali metal element) and SiO2 and has a molar ratio of SiO2 to the alkali metal oxide of 2.3 or more. The carbon-containing refractory is used at a high temperature of 400° C. or more and contains 1 mass % or more of carbon or a carbon compound.
机译:提供一种用于抑制背面氧化的方法和衬里结构,由此获得高的气密性和抑制背面氧化的巨大效果。抑制含碳耐火材料的背面氧化的方法包括通过在背面上施加碱金属硅酸盐水溶液并使该碱金属硅酸盐水溶液固化而在含碳耐火材料的背面上形成粘附层。碱金属硅酸盐水溶液包含碱金属氧化物R 2 O(R为碱金属元素)和SiO 2 ,且摩尔比为SiO 2 为2.3或更高的碱金属氧化物。含碳耐火材料在400℃以上的高温下使用,并且含有1质量%以上的碳或碳化合物。

著录项

  • 公开/公告号US10183895B2

    专利类型

  • 公开/公告日2019-01-22

    原文格式PDF

  • 申请/专利权人 JFE STEEL CORPORATION;

    申请/专利号US201515110803

  • 发明设计人 AKIHIKO INOUE;YOSHISATO KIYOTA;

    申请日2015-01-06

  • 分类号C04B41/50;C04B41/85;C04B41/00;F27D1/00;B05D7/00;

  • 国家 US

  • 入库时间 2022-08-21 12:11:55

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号