process for the production of foundry moulds, especially stratified foundry moulds for foundries precision, is making layers of liquid ceramic paste on model casting, drying and subsequent layers of form removal model and firing forms.way is characterized by the fact that at least one layer made of liquid ceramic paste containing binder and composition for loose materials consisting in% by weight of 20 to 65% ceramic material, 8 - 20% of a reactive metal, preferably al about grain size 0 - 0, 3 mm, 25 - 60% of metal oxides, preferably fe2o3 or fe3o4,0 - 10% activators exothermic reaction kclo4 favourably, and / or nano3 and / or kno3 and / or stop almg, whereby the quantity of binder composition contains quantities of loose materials within 1: 0.75 to 1: 4.5, and then after the removal model and after drying, the form is heated to temperatures y initiate exothermic reaction, and thereafter, cooling to form.the glue is aqueous or hydroalcoholic or aqueous acetone solution containing tlenkowu0105 colloidal substance, preferably sio2 or al2o3 or zro2.
机译:铸造模具,特别是分层铸造模具的生产方法,用于铸造精度,是在模型铸造,干燥以及随后的脱模模型和烧成模型层上制造液体陶瓷浆料层。该方法的特征在于至少一层由含有粘合剂的液态陶瓷浆料和用于散装材料的组合物制成,该组合物由重量百分比为20%至65%的陶瓷材料,8%至20%的活性金属组成,最好是大约0-0、3 mm,25-60%的晶粒度金属氧化物,最好是fe2o3或fe3o4,0-10%的活化剂有利地放热反应kclo4,和/或nano3和/或kno3和/或终止镁,由此粘合剂组合物的量包含1范围内的松散材料: 0.75至1:4.5,然后在去除模型后干燥后,将模板加热至温度y引发放热反应,然后冷却以形成胶。胶水为含水或水醇或丙酮水溶液,含有胶体物质,优选sio2或al2o3或zro2。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号