the object of the application is the way bioaktywnej coating calcium phosphate deposition on nickel - titanium alloy element made in a shape memory effect.so obtained may find application in particular elements as medical implants.the way is that the water bath octanowej, ph neutral, which consists of 00167m to 0030m c4h6cao4 from 0,01 to 0018m (nh4) hpo4 from 0,01 to 0,05m c6h8o7 and from 0.037m to 0074m nh4cl, introduces an element made of nickel titanium memory alloy showing the shape, preferably the composition ru00f3wnoatomowym,constituting the electrode ni - ti and held in bath, preferably at room temperature, until the stabilising potential electrodes, ni - tithen subjected her elektroredukcji process from solution, carried out in the same water bath octanowej, preferably at room temperature.the potential of selected range - 1.5 to - 10 v potential circuit opened the eoc in time from 10 to 45 minutes.
机译:该应用的目的是通过生物合金在形状记忆效应的镍-钛合金元素上涂覆磷酸钙沉积物的方法。因此获得的结果可能在医疗植入物等特定元素中得到应用。该方法是水浴octanowej,ph中性,它由从0.001到0018m的c4h6cao4从0.01到0018m(nh4)的hpo4从0.01到0.05m c6h8o7和从0.037m到0074m nh4cl组成,引入了一种镍钛记忆合金制成的元素,其形状,形状,优选成分r,将电极ni -ti并保持在浴中,优选在室温下进行,直到稳定电位电极,ni-tithen从溶液中进行她的elektroredukcji过程,在相同的水浴中,优选在室温下进行。选定范围的电位-1.5至-10 V电位电路在10至45分钟的时间内打开了EOC。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号