The present utility model relates to fiberboard but more particularly to banana and oil palm fiberboard comprising of 0.50 - 0. 70 kg. of oil palm frond 0.30- 0.50 kg. of banana pseudo stem, mixed with about 0.25 kg. of used paper pulp and 0.1 0 kg. of cassava starch. The said fiberboard wherein the mixture is consisting of 0.40 kg. banana pseudo stem, 0.60 kg. oil palm frond, 0.25 kg. used paper pulp and 0.10 kg. cassava starch obtained the highest weight density of 0.339 g/cm3 and the greatest flexural strength of 86.76 MPa.