Described are processes for shaping age hardenable aluminum alloys, such as 2XXX, 6XXX and 7XXX aluminum alloys in T4 temper, or articles made of such alloys, including aluminum alloy sheets. The processes involve heating the sheet or article before and/or concurrently with a forming step. The sheet is heated to a specified temperature in the range of 100-600°C at a specified heating rate within the range of 3-600°C/s, for example 3-90°C/s. Such a combination of temperature and heating rate results in an advantageous combination of sheet properties.