首页> 外国专利> METHOD FOR RECOVERING VALUABLE COMPONENTS FROM MIXED SLAG CONTAINING COPPER AND IRON

METHOD FOR RECOVERING VALUABLE COMPONENTS FROM MIXED SLAG CONTAINING COPPER AND IRON

机译:从含铜铁渣中回收有价值成分的方法

摘要

Provided is a method for recovering valuable components from mixed slag containing copper and iron, which comprises S1, mixing slag; adding copper slag into a smelting reaction device, and simultaneously adding one or more of lead smelting slag, blast furnace slag, steel slag and ferroalloy slag to form mixed slag; heating the molten slag to a molten state to form reaction molten slag, mixing evenly, meeting the requirements that the temperature of the molten slag is 1050-1450℃ and the alkalinity CaO/SiO2 ratio of the molten slag is equal to 0.15-1.5, to obtain the reacted molten slag; S2, separating and recycling. The recovery of copper, iron, zinc, lead, gold and silver in non-ferrous metallurgical slag and iron and steel metallurgical slag is realized, and the problems of large accumulation of slag and environmental pollution at present are solved.
机译:提供一种从含铜铁混合渣中回收有价值成分的方法,该方法包括S1混合渣。向熔炼反应装置中加入铜渣,同时加入铅熔渣,高炉渣,钢渣和铁合金渣中的一种或多种,​​形成混合渣。将熔渣加热至熔融状态,形成反应熔渣,均匀混合,满足熔渣温度为1050-1450℃,碱度CaO / SiO 2 比的要求炉渣等于0.15-1.5,得到反应后的熔融炉渣。 S2,分离和回收。实现了有色冶金渣和钢铁冶金渣中铜,铁,锌,铅,金,银的回收,解决了目前渣量大,环境污染的问题。

著录项

  • 公开/公告号WO2019071794A1

    专利类型

  • 公开/公告日2019-04-18

    原文格式PDF

  • 申请/专利权人 NORTHEASTERN UNIVERSITY;

    申请/专利号WO2017CN115649

  • 发明设计人 ZHANG LI;ZHANG WU;

    申请日2017-12-12

  • 分类号C22B7/04;C21B3/06;

  • 国家 WO

  • 入库时间 2022-08-21 11:55:16