A highly crystalline Cu-containing KFI zeolite and a process for its preparation are provided. The highly crystalline Cu-containing KFI zeolite contains Cu and Al 2 , and the Cu / Al 2 molar ratio is 40 to 80%. The process for preparing the highly crystalline Cu-containing KFI zeolite comprises the steps of preparing a base zeolite, preparing a metal cation and a hydroxide ion solution, mixing the base zeolite and the solution to form a zeolite mixture, Heating to form a crystallized zeolite, and providing Cu to the crystallized zeolite.
机译:提供了一种高度结晶的含铜KFI沸石及其制备方法。高结晶度的含铜KFI沸石含有Cu和Al 2 ,Cu / Al 2 摩尔比为40〜80%。制备高度结晶的含铜KFI沸石的方法包括以下步骤:制备基础沸石,制备金属阳离子和氢氧根离子溶液,将基础沸石和溶液混合以形成沸石混合物,加热以形成结晶沸石。 ,并向结晶沸石中提供Cu。

著录项

  • 公开/公告号KR101928183B1

    专利类型

  • 公开/公告日2018-12-11

    原文格式PDF

  • 申请/专利权人 서울대학교산학협력단;

    申请/专利号KR20170054322

  • 发明设计人 김도희;김종현;

    申请日2017-04-27

  • 分类号B01J29/76;B01J29/70;B01J35/10;B01J37;B01J37/30;

  • 国家 KR

  • 入库时间 2022-08-21 11:52:02

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号