The present invention relates to a manufacturing method for a neutral sintered manganese ore with excellent usability in a ferromanganese electric furnace and a neutral sintered manganese ore manufactured by the same. According to the present invention, the manufacturing method for a neutral sintered manganese ore includes: a step of obtaining a neutral mixed fine ore which is a mixture of basic manganese fire ore and an acidic manganese fine ore, by mixing the basic manganese fine ore and the acidic manganese fine ore so that a weight ratio of CaO/SiO_2 is in a ratio of 0.5-2.0 after being sintered; and a sintering step. According to the present invention, a basicity ratio of the neutral sintered manganese ore is optimized, and the neutral sintered manganese ore is suitable to be used for the ferromanganese electric furnace. According to the present invention, the Fe element ratio of the neutral sintered manganese ore is optimized. So, the neutral sintered manganese ore is suitable to be used for the ferromanganese electric furnace.
机译:本发明涉及一种在铁锰电炉中具有优异的可用性的中性烧结锰矿的制造方法以及由其制造的中性烧结锰矿。根据本发明,中性烧结锰矿石的制造方法包括:通过将碱性锰细矿石与碱性锰细矿石混合而获得中性混合细矿石的步骤,所述中性混合细矿石是碱性锰火矿石和酸性锰细矿石的混合物。酸性锰矿粉,烧结后CaO / SiO_2的重量比为0.5〜2.0。和烧结步骤。根据本发明,中性烧结锰矿的碱度比被优化,并且中性烧结锰矿适合用于铁锰电炉。根据本发明,优化了中性烧结锰矿石的Fe元素比率。因此,中性烧结锰矿适用于铁锰电炉。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号