Disclosed are a method for manufacturing a hot rolled steel sheet for an oil well tube and a hot rolled steel sheet manufactured thereby. In one embodiment, the method for manufacturing a hot rolled steel sheet for oil wells includes: carbon (C): 0.2 to 0.3 wt%, silicon (Si): more than 0 and 0.25 wt% or less, manganese (Mn): 1.15 to 1.55 wt%, aluminum (Al) : 0.01 to 0.05 weight%, phosphorus (P): more than 0 and 0.018 weight% or less, sulfur (S): more than 0 and 0.005 weight% or less, nitrogen (N): more than 0 and 0.006 weight% or less, and residual amount of iron (Fe) Reheating the steel slab containing the steel and other unavoidable impurities; Manufacturing a hot rolled sheet by hot rolling the reheated steel slab under a finish rolling temperature of 800 ° C. to 850 ° C .; And winding the hot rolled sheet material to a winding temperature: 600 to 660 ° C.
机译:公开了一种用于油井管的热轧钢板的制造方法以及由此制造的热轧钢板。在一个实施例中,一种用于油井的热轧钢板的制造方法包括:碳(C):0.2至0.3wt%,硅(Si):大于0且小于或等于0.25wt%,锰(Mn):1.15至1.55重量%,铝(Al):0.01至0.05重量%,磷(P):大于0至0.018重量%以下,硫(S):大于0至0.005重量%以下,氮(N) :大于0且小于或等于0.006重量%,以及铁(Fe)的残留量对含有钢和其他不可避免的杂质的钢坯进行加热。通过在800℃至850℃的终轧温度下对再加热的钢坯进行热轧来制造热轧板。并将热轧板料卷绕至卷绕温度:600至660℃。

著录项

  • 公开/公告号KR102021197B1

    专利类型

  • 公开/公告日2019-09-11

    原文格式PDF

  • 申请/专利权人 현대제철 주식회사;

    申请/专利号KR20170156278

  • 发明设计人 신지웅;권태우;유용재;최종민;

    申请日2017-11-22

  • 分类号C21D8/02;B21B3/02;B21B37/74;C21D9/46;C22C38/04;C22C38/06;

  • 国家 KR

  • 入库时间 2022-08-21 11:47:45

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号