The present invention relates to a process for producing a grain of sintered magnesia, wherein the sintered magnesia is prepared by sintering pellets, in particular pellets, from MgO flour, preferably from MgO powder, and then mechanically crushing the pellets, sintering in such a way the grain has a grain porosity (total porosity) according to DIN EN 993-1: 1195-04 and DIN EN 993-18: 1999-01 of 15 to 38% by volume, preferably of 20 to 38% by volume, and an offset for producing a coarse ceramic, refractory, shaped or unshaped product containing the porous sintered magnesia, such a product made from the batch, and a method for the production thereof, a lining, in particular a working lining and / or a back wall, of a large-capacity industrial furnace, wherein the Delivery, in particular the working food and / or the Hintermauerung, at least one such product on shows, as well as such an industrial furnace.
机译:本发明涉及一种生产烧结氧化镁的方法,其中该烧结氧化镁是通过以下方法制备的:烧结粒料,特别是从MgO粉,优选地从MgO粉中烧结粒料,然后机械粉碎粒料,以这种方式烧结根据DIN EN 993-1:1195-04和DIN EN 993-18:1999-01,该颗粒具有15至38体积%,优选20至38体积%的晶粒孔隙度(总孔隙度),并且用于生产包含多孔烧结氧化镁的粗陶​​瓷,耐火材料,成形或未成形产品的胶印品,这种由批料制成的产品,及其生产方法,衬里,特别是工作衬里和/或后壁,一种大容量工业炉,其中,交付物,特别是工作食品和/或Hintermauerung,至少有一种这样的产品在展示,以及这种工业炉。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号