首页> 外国专利> PROCESS FOR PREPARING A HIERARCHIC ZEOLITE CATALYST FOR THE AROMATISATION OF C5 TO C9 ALKANES

PROCESS FOR PREPARING A HIERARCHIC ZEOLITE CATALYST FOR THE AROMATISATION OF C5 TO C9 ALKANES

机译:制备用于C5到C9烷烃芳构化的分层沸石催化剂的方法

摘要

A process for preparing a hierarchical zeolite catalyst for aromatization of C5-C9 alkane that provides high conversion percentage of precursor to yields and high aromatics selectivity, wherein said process comprises the following steps: (a) preparing a solution containing alumina compound, silica compound, and soft template; (b) subjecting the mixture obtained from step (a) to hydrothermal process at determined time and temperature to form said mixture into the hierarchical zeolite; (c) contacting the hierarchical zeolite obtained from step (b) with ammonium salt solution; and (d) contacting the hierarchical zeolite obtained from step (c) with gallium salt solution; wherein the soft template in step (a) is a quaternary phosphonium salt in which the mole ratio of the silica compound to the alumina compound in step (a) is in a range of 20 to 120 and the gallium salt in step (d) has gallium to zeolite ratio in a range of 0.5 to 5 % by weight.
机译:一种制备用于C5-C9烷烃芳构化的分级沸石催化剂的方法,该方法可提供高产率的前驱体转化率和高的芳烃选择性,其中所述方法包括以下步骤:(a)制备含氧化铝化合物,二氧化硅化合物的溶液,和软模板; (b)在确定的时间和温度下将由步骤(a)获得的混合物进行水热处理,以将所述混合物形成分级沸石; (c)使从步骤(b)获得的分级沸石与铵盐溶液接触; (d)使由步骤(c)得到的分级沸石与镓盐溶液接触;其中步骤(a)中的软模板是季phospho盐,其中步骤(a)中的二氧化硅化合物与氧化铝化合物的摩尔比为20至120,并且步骤(d)中的镓盐具有镓与沸石的比例为0.5-5重量%。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号