A method for manufacturing a metal sheet with a ZnAl coating and with optimised drying, corresponding metal sheet, part and vehicle

机译:一种具有ZnAl涂层和优化干燥的金属板的制造方法,相应的金属板,零件和车辆

摘要

The present invention provides a method for manufacturing a metal sheet. In this method, at least one of the following equations is satisfied: Z d + 18   ln  ( Z d ) 8   ln  ( P V ) - 27.52 ( A ) fO 2 2.304 · 10 - 3 ( 27.52 + Z d + 8   ln  ( V P  ( Z d ) 2.25 ) ) 2 ( B ) wherein: Z is the distance between the metal sheet and the nozzle along the main ejection direction (E), Z being expressed in mm, d is the average height of the outlet of the nozzle along with the running direction of the metal sheet in front of the nozzle, d being expressed in mm, V is the running speed of the metal sheet in front of the nozzle, V being expressed in m·s1, P is the pressure of the wiping gas in the nozzle, P being expressed in N·m2, and fO2 is the volume fraction of oxygen in the wiping gas. A metal sheet, part and land motor vehicle are also provided.
机译:本发明提供一种金属板的制造方法。在该方法中,至少满足以下等式之一:Z d + 18 ln ln(Z d)<8 ln ln(PV)-27.52(A)fO 2 <2.304·10-3(27.52 + Z d + 8 ln(VP(Z d)2.25))2(B)其中:Z是金属板和喷嘴之间沿主喷射方向(E)的距离,Z以毫米表示,d是喷嘴出口的平均高度以及喷嘴前面的金属板的行进方向,d以毫米表示,V是喷嘴前面的金属板的行进速度,V为用m·s1表示,P是喷嘴内擦拭气体的压力,P是N·m2表示,fO2是擦拭气体中氧气的体积分数。还提供了金属板,零件和陆地机动车辆。

著录项

  • 公开/公告号GB201817647D0

    专利类型

  • 公开/公告日2018-12-12

    原文格式PDF

  • 申请/专利权人 ARCELORMITTAL;

    申请/专利号GB20180017647

  • 发明设计人

    申请日2014-02-10

  • 分类号C23C2/06;C23C2/20;C23C2/26;

  • 国家 GB

  • 入库时间 2022-08-21 11:43:39

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号